Structural, morphological and electrophysical properties of Sb2Se3 films obtained at different temperatures of the selenium source
DOI:
https://doi.org/10.52304/.v24i3.360Keywords:
electrical conductivity, morphological properties, selenium source temperature, Sb2Se3, stoichiometric compositionAbstract
Sb2Se3 crystalline films were obtained by chemical molecular beam deposition (CMBD) from separate sources of the Sb2Se3 binary compound and the Se element, at a substrate temperature of 500°С. The main strong peaks (221), (211) and secondary weak peaks (020), (120) and (310) are observed on the X-ray patterns, which noticeably change with the Se temperature. At
a selenium source temperature of 430°C, the grains larger than 4 µm are observed on the Sb2Se3 film surface, and rod-like grains of Sb2Se3 appeared. The Sb2Se3 films were Sedeficient at a selenium source temperature of 350°C, and with a further increase in the selenium source temperature, approached the stoichiometric composition. It is shown that Sb2Se3 films close to the stoichiometric composition with the ratio Sb/Se 0.68 are obtained at a selenium source temperature of 430°C. The specific electrical conductivities of Sb2Se3 films range from σ=9×10−5 (Ohm·cm)−1 to σ=6×10−4 (Ohm·cm)−1 depending on the technological regime.